Steps for making media balls for silver ore mine mineral processing
Jul 11, 2019
The molten iron is subjected to a fine flow casting at a temperature of 1340 ° C to 1390 ° C; after cooling for 4 hours to 5 hours, the mold is opened, the cast iron balls are taken out; the cooled cast iron balls are ground; the polished cast iron balls are put into a heating furnace, and the temperature is raised. 550 ° C ~ 650 ° C, heat for 3 hours to 4 hours; quenched in the oil pool, the temperature is 870 ° C ~ 950 ° C, 45 minutes after air cooling to room temperature, and then put into the furnace; tempering 4 hours to 6 hours, temperature From 175 ° C to 195 ° C, after cooling to room temperature, the finished product is obtained.
The media balls for silver ore mine mineral processing adds rare earth element Ce to the cast iron. Since Ce is re-dispersed by solute during solidification, it is enriched in the primary austenite front melt, which refines the primary austenite; Activated adsorption on the growing eutectic carbide, which promotes the increase of eutectic subcooling and the eutectic solidification range, which significantly improves the cast iron eutectic structure, and its mechanical properties are above HRC60, and the impact toughness is above 3.9J/cm2. The obtained product has good impact resistance, does not break during use, and has a long service life.
Adding Nb and B to the cast iron improves the hardness and wear resistance of the media balls for silver ore mine mineral processing. The proper amount of B and Cu can improve the hardenability of the matrix. Cu and Nb are beneficial to refine the grains and increase the strength of the matrix. Impact toughness and corrosion resistance.
www.grindingballsmedia.com