Analysis of out-of-round and eccentric wear of Grinding Media Balls (3)

Oct 31, 2021

The problem of the gradation ratio of the mill. Although there will be steel ball specifications ranging from 60 to 120mm in the mill, only one kind of steel ball material is used, such as: a mill has four grades of steel balls, namely 120mm, 100mm, 80mm, and 60mm , And all use a kind of B2 material, which will cause very low wear at the beginning of the mill operation, but after 30-40 days of operation, as the time becomes longer and longer, the number of steel balls added continues to increase, and the wear of the steel balls There will be a lot of fluctuations, not only the increase in wear is obvious, but also the out-of-round rate of the steel ball will increase, and the frequency of eccentric wear will increase, and it is very obvious (this will be introduced separately).

https://www.grindingballsmedia.com/